Skip to content

Latest commit

 

History

History
170 lines (114 loc) · 10.5 KB

File metadata and controls

170 lines (114 loc) · 10.5 KB

Multimodal - Weld Defect Detection

MultiModal Weld Defect Detection sample application demonstrates how to use AI at the edge to identify defects in manufacturing environments by analyzing both image and time series sensor data.

If you want to start working with it, check out the Get Started Guide or How-to Guides for Multimodal applications.

How It Works

MultiModal Weld Defect Detection Architecture Diagram

Data flow explanation

As seen in the architecture diagram above, the sample app at a high-level comprises of a data simulator, analytics and visualization components. Below is an explanation of how this architecture translates to data flow in the weld defect detection use case.

1. Weld Data Simulator

The Weld Data Simulator uses sets of time synchronized .avi and .csv files from the edge-ai-suites/manufacturing-ai-suite/industrial-edge-insights-multimodal/weld-data-simulator/simulation-data/ subset of test dataset coming from Intel_Robotic_Welding_Multimodal_Dataset. It ingests the .avi files as RTSP streams via the mediamtx server. This enables real-time video ingestion, simulating camera feeds for weld defect detection. Similarly, it ingests the .csv files as data points into Telegraf using the MQTT protocol.

2. Analytics Modules

2.1 DL Streamer Pipeline Server

The DL Streamer Pipeline Server microservice reads the frames/images from the MediaMTX server over RTSP protocol, runs the configured DL weld defect classification model, publishes the frame metadata results over MQTT, stores the processed frames in SeaweedFS S3 storage, and generates the WebRTC stream with bounded boxes for visualization in Grafana.

DL Streamer Pipeline Server config.json

Pipeline Configuration:

Key Description Example Value
name The name of the pipeline configuration. "weld_defect_classification"
source The source type for video ingestion. "gstreamer"
queue_maxsize Maximum size of the queue for processing frames. 50
pipeline GStreamer pipeline string defining the video processing flow from RTSP source through classification to output. "rtspsrc add-reference-timestamp-meta=true location=\"rtsp://mediamtx:8554/live.stream\" latency=100 name=source ! rtph264depay ! h264parse ! decodebin ! videoconvert ! video/x-raw,format=BGR ! gvaclassify inference-region=full-frame name=classification ! gvawatermark ! gvametaconvert add-empty-results=true add-rtp-timestamp=true name=metaconvert ! queue ! gvafpscounter ! appsink name=destination"
parameters Configuration parameters for pipeline elements, specifically for the classification element properties. See below for nested structure

Parameters Properties:

Key Description Value
classification-properties Properties for the classification element in the pipeline. Object containing element configuration
element.name Name of the GStreamer element to configure. "classification"
element.format Format type for element properties. "element-properties"

Destination Configuration:

The destination key contains two main properties:

  • metadata - defines where to send inference results
  • frame - an array defining one or more video output destinations

Metadata (destination.metadata):

Publishes inference results via MQTT.

Key Description Example Value
metadata.type The protocol type for sending metadata information. "mqtt"
metadata.topic The MQTT topic where vision classification results are published. "vision_weld_defect_classification"

Frame Destinations (destination.frame):

An array defining one or more video output destinations. Each entry requires a type field.

WebRTC Streaming (type: "webrtc"):

Key Description Example Value
type Frame destination type. "webrtc"
peer-id Unique identifier for the WebRTC peer connection. "samplestream"

S3 Storage (type: "s3_write"):

Key Description Example Value
type Frame destination type. "s3_write"
bucket S3 bucket name for storing processed frames. "dlstreamer-pipeline-results"
folder_prefix Directory path within the bucket for storing frames. "weld-defect-classification"
block Controls S3 write synchronization with MQTT publishing. When false, metadata may arrive before S3 write completes. When true, MQTT metadata is sent only after S3 write completion. false
2.2 Time Series Analytics Microservice

Time Series Analytics Microservice uses Kapacitor - a real-time data processing engine that enables users to analyze time series data. It reads the weld sensor data points point by point coming from Telegraf, runs the ML CatBoost model to identify the anomalies, writes the results into configured measurement/table in InfluxDB and publishes anomalous data over MQTT. Also, publishes all the processed weld sensor data points over MQTT.

The UDF deployment package used for weld data is available at edge-ai-suites/manufacturing-ai-suite/industrial-edge-insights-multimodal/config/time-series-analytics-microservice. Directory details is as below:

config.json

UDFs Configuration:

The udfs section specifies the details of the UDFs used in the task.

Key Description Example Value
name The name of the UDF script. "weld_anomaly_detector"
models The name of the model file used by the UDF. "weld_anomaly_detector.cb"

Note: The maximum allowed size for config.json is 5 KB.

Alerts Configuration:

The alerts section defines the settings for alerting mechanisms, such as MQTT protocol.

MQTT Configuration:

The mqtt section specifies the MQTT broker details for sending alerts.

Key Description Example Value
mqtt_broker_host The hostname or IP address of the MQTT broker. "ia-mqtt-broker"
mqtt_broker_port The port number of the MQTT broker. 1883
name The name of the MQTT broker configuration. "my_mqtt_broker"
udfs/

Contains the python script to process the incoming data. Uses CatBoostClassifier machine learning algorithm from the CatBoost library to run on CPU to detect anomalous weld data points using sensor data.

Note: Please note, CatBoost models don't run on Intel GPUs.

tick_scripts/

The TICKScript weld_anomaly_detector.tick determines processing of the input data coming in. Mainly, has the details on execution of the UDF file, storage of processed data and publishing of alerts. By default, it is configured to publish the alerts to MQTT.

models/

The weld_anomaly_detector.cb is a model built using the CatBoostClassifier Algo of CatBoost ML library.

2.3 Fusion Analytics

Fusion Analytics subscribes to the MQTT topics coming out of DL Streamer Pipeline Server and Time Series Analytics Microservice, applies AND/OR logic to determine the anomalies during weld process, publishes the results over MQTT and writes the results as a measurement in InfluxDB It also stores the vision metadata from the DL Streamer Pipeline Server as a measurement in InfluxDB.

3. Data Storage

InfluxDB stores the incoming data coming from Telegraf, Time Series Analytics Microservice and Fusion Analytics .

4. Data Visualization

Grafana provides an intuitive user interface for visualizing time series data stored in InfluxDB and also rendering the output of DL Streamer Pipeline Server coming as WebRTC stream. Additionally, it visualizes the fusion analytics results stored in InfluxDB.

Next Steps

Refer to the detailed instructions in Get Started.